Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 0.758 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.758 - 24.8 MPa
110 - 3600 psi
Average value: 15.5 MPa Grade Count:490
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Tensile Strength, Ultimate 0.758 MPa
110 psi
cured 8 hours @ 93°C
Abatron AboCast/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Tensile Strength, Ultimate 0.758 MPa
110 psi
ASTM D638
Colorite Polymers Vinylbond 96-1203-40 Compound
Description: Vinylbond 96-1203-40 is a flexible vinyl extrusion compound formulated specifically for the window market industry. This particular compound offers excellent bonding characteristics to ..