Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 301-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 90.0 J | 66.4 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4310-6 Polycarbonate EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ.. |
|||
Dart Drop, Total Energy | 90.0 J | 66.4 ft-lb | 8000 ipm; ASTM D3763 |
Styron CALIBREâ„¢ 2060-6 Polycarbonate CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity.. |
|||
Dart Drop, Total Energy | 90.0 J | 66.4 ft-lb | 8000 ipm; ASTM D3763 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 303-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 90.0 J | 66.4 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Dart Drop, Total Energy | 90.0 J @Thickness 3.20 mm |
66.4 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |