Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® OQ3820 PC High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Asia Pacific) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Dart Drop, Total Energy | 85.0 J @Temperature 23.0 °C |
62.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |