Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing, Flame Retardant... |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10312 PA (Asia Pacific) 9X10312 is 50% glass fiber reinforced, impact modified nylon material. High modulus, high flow and good ductility, Low Moisture Absorption. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific) LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LZZ PES LNP THERMOCOMP* JF006LZZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Extrusion Grade, Low Extractable. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC (Asia Pacific) LNP* Stat-kon* DEL339XF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant,.. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6 LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
3000N, 6.3mm deflection; ISO 6603 |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
3200N, 6mm deflection; ISO 6603 |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Dart Drop, Total Energy | 12.0 J | 8.85 ft-lb | ISO 6603-1 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Dart Drop, Total Energy | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP VERTON MV006BS PP LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl.. |