Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 2.00 - 10.0 J | 1.48 - 7.38 ft-lb | Average value: 4.67 J Grade Count:3 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Dart Drop, Total Energy | 8.00 - 10.0 J | 5.90 - 7.38 ft-lb | Average value: 9.00 J Grade Count:6 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |