Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 67.8 J | 50.0 ft-lb | BASF |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |
|||
Dart Drop, Total Energy | 67.8 - 285 J | 50.0 - 210 ft-lb | Average value: 204 J Grade Count:4 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |