Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 67.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 915R PC
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific)
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific)
Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties..
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific)
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
Dart Drop, Total Energy 67.0 J

@Temperature -20.0 °C
49.4 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FL2000 PC
Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa..
Dart Drop, Total Energy 67.0 J
49.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics ULTEM D9065 PEI
Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Dart Drop, Total Energy 67.0 J
49.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics ULTEM D9065 PEI (Asia Pacific)
Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East)
25 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 67.0 J

@Temperature 23.0 °C
49.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized