Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature -30.0 °C |
45.0 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature -30.0 °C |
45.0 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific) Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | SABIC Method |
SABIC Innovative Plastics FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 505R PC Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2010 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® EM1210 PC Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® FL403 PC Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"". |
|||
Dart Drop, Total Energy | 61.0 J | 45.0 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP COLORCOMP DX98735H PC LNP* COLORCOMP* DX98735H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare. |
|||
Dart Drop, Total Energy | 61.0 J @Thickness 3.17 mm, Temperature 22.8 °C |
45.0 ft-lb @Thickness 0.125 in, Temperature 73.0 °F |
7.5MPH; ASTM D3763 |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Dart Drop, Total Energy | 61.0 J @Temperature -30.0 °C |
45.0 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Dart Drop, Total Energy | 61.0 J @Temperature -30.0 °C |
45.0 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Dart Drop, Total Energy | 61.0 J @Temperature -30.0 °C |
45.0 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |