Polymer Property : Dart Drop, Total Energy = 50.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 67.8 J
50.0 ft-lb
BASF
BASF Ultramid® 8281 HS GP PA6 (Dry)
Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p..
Dart Drop, Total Energy 67.8 - 285 J
50.0 - 210 ft-lb
Average value: 204 J Grade Count:4
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..