Polymer Property : Dart Drop, Total Energy = 43.5 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 59.0 J
43.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® LUX7189 PC
Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems.
Dart Drop, Total Energy 59.0 J
43.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® LUX7189 PC (Europe-Africa-Middle East)
Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems.
Dart Drop, Total Energy 59.0 J

@Temperature 23.0 °C
43.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXM941A PC
PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance.
Dart Drop, Total Energy 59.0 J

@Temperature -40.0 °C
43.5 ft-lb

@Temperature -40.0 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Dart Drop, Total Energy 59.0 J

@Temperature -40.0 °C
43.5 ft-lb

@Temperature -40.0 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Dart Drop, Total Energy 59.0 J

@Temperature -40.0 °C
43.5 ft-lb

@Temperature -40.0 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Dart Drop, Total Energy 59.0 J
43.5 ft-lb
ASTM D3763
Styron EMERGEâ„¢ 8600-10 Polycarbonate
EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental ..