Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 520 J @Thickness 3.20 mm |
384 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1080-70 Polycarbonate Resin Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Ch.. |