Polymer Property : Dart Drop, Total Energy = 380 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 380 J

@Temperature 23.0 °C
280 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.