Mechanical Properties Metric English Comments
Dart Drop, Total Energy 47.5 J
35.0 ft-lb
Conditioned; ASTM D3763
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better ..
Dart Drop, Total Energy 47.5 J
35.0 ft-lb
Instrumented; ASTM D3763
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..