Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 44.0 J | 32.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Dart Drop, Total Energy | 44.0 J | 32.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Dart Drop, Total Energy | 44.0 J | 32.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Dart Drop, Total Energy | 44.0 J @Temperature 23.0 °C |
32.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PN275 PPE+PS PPE+PS with low mineral loading. High heat, platable applications. |
|||
Dart Drop, Total Energy | 44.0 J @Temperature 23.0 °C |
32.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PN275F PPE+PS PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications. |