Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 120 J @Temperature 23.0 °C |
88.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dart Drop, Total Energy | 120 J @Temperature 23.0 °C |
88.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dart Drop, Total Energy | 120 J @Temperature 23.0 °C |
88.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |