Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 1.48 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP FARADEX PS003E PA 6
LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A..
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 2.00 - 10.0 J
1.48 - 7.38 ft-lb
Average value: 4.67 J Grade Count:3
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Dart Drop, Total Energy 2.00 - 16.0 J
1.48 - 11.8 ft-lb
Average value: 9.54 J Grade Count:13
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12
LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS
LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66
LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific)
LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP UL002S PPA
LNP* LUBRICOMP* UL002S is a compound based on Polyphthalamide resin containing 10% PTFE. Added features of this grade include: Heat Stabilized, Wear Resistant.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT
LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific)
LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI
LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12
LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr..
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON SD000 PA12
LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer
LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific)
LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66
LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA
LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Asia Pacific)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DX05305C PC
LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Dart Drop, Total Energy 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66
LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads.
Dart Drop, Total Energy 2.00 - 30.7 J

@Temperature -20.0 - 0.000 °C
1.48 - 22.6 ft-lb

@Temperature -4.00 - 32.0 °F
Average value: 12.7 J Grade Count:2
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..
Dart Drop, Total Energy 2.00 - 380 J
1.48 - 280 ft-lb
Average value: 29.0 J Grade Count:158
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON LX04420C PEEK
LNP* STAT-KON* LX04420C is a compound based on Polyetheretherketone resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding Syst..
Copyright © lookpolymers.com All Rights Reserved