Mechanical Properties Metric English Comments
Ball Indentation Hardness 220 MPa

@Load 36.5 kg
31900 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Ball Indentation Hardness 220 MPa

@Load 36.5 kg
31900 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Ball Indentation Hardness 220 MPa

@Load 36.5 kg
31900 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced
20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following ..
Ball Indentation Hardness 220 MPa

@Load 36.5 kg
31900 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..