Mechanical Properties Metric English Comments
Ball Indentation Hardness 120 MPa

@Load 36.5 kg
17400 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Ball Indentation Hardness 120 MPa

@Load 36.5 kg
17400 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Ball Indentation Hardness 120 MPa

@Load 36.5 kg
17400 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Ball Indentation Hardness 120 MPa

@Load 36.5 kg
17400 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Ball Indentation Hardness 120 MPa

@Load 36.5 kg
17400 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced
20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following ..
Ball Indentation Hardness 120 MPa

@Load 36.5 kg
17400 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties..