Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 6.14 kN/m @Temperature 24.0 °C, Time 259000 sec |
35.0 pli @Temperature 75.2 °F, Time 72.0 hour |
canvas/canvas |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 6.14 kN/m @Temperature 14.0 °C, Time 1.21e+6 sec |
35.0 pli @Temperature 57.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 6.14 kN/m @Temperature 14.0 °C, Time 1.21e+6 sec |
35.0 pli @Temperature 57.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 6.14 kN/m @Temperature 38.0 °C |
35.0 pli @Temperature 100 °F |
180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 6.14 kN/m @Temperature 23.0 °C |
35.0 pli @Temperature 73.4 °F |
180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 6.14 kN/m @Temperature 65.0 °C |
35.0 pli @Temperature 149 °F |
180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 6.14 kN/m @Temperature 24.0 °C, Time 259000 sec |
35.0 pli @Temperature 75.2 °F, Time 72.0 hour |
canvas/canvas |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 6.14 kN/m @Temperature 24.0 °C, Time 605000 sec |
35.0 pli @Temperature 75.2 °F, Time 168 hour |
180°, Canvas/Steel |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Peel Strength | 6.14 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec |
35.0 pli @Temperature 75.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Peel Strength | 6.14 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec |
35.0 pli @Temperature 75.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4475 Industrial Adhesive Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer.. |
|||
Peel Strength | 6.14 kN/m @Temperature 14.0 °C, Time 1.21e+6 sec |
35.0 pli @Temperature 57.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |