Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.00150 kN/m @Time 0.000 sec |
0.00856 pli @Time 0.000 hour |
180° peel, peel speed is 100 mm/min |
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Peel Strength | 0.00150 kN/m @Time 3.24e+6 sec |
0.00856 pli @Time 900 hour |
180° peel, peel speed is 100 mm/min |
Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |