Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.00115 kN/m @Time 2.88e+6 sec |
0.00656 pli @Time 800 hour |
180° peel, peel speed is 100 mm/min |
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |