Mechanical Properties Metric English Comments
Tensile Strength 40.0 MPa

@Strain 2.00 %,
Temperature 80.0 °C
5800 psi

@Strain 2.00 %,
Temperature 176 °F
50mm/min
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Tensile Strength 40.0 MPa

@Strain 2.00 %,
Temperature 150 °C
5800 psi

@Strain 2.00 %,
Temperature 302 °F
5mm/min
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength 40.0 MPa

@Temperature 70.0 °C
5800 psi

@Temperature 158 °F
5mm/min (0.2in/min); ASTM D638
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..
Tensile Strength 40.0 MPa

@Strain 3.00 %,
Temperature 60.0 °C
5800 psi

@Strain 3.00 %,
Temperature 140 °F
ISO 527
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing
Tensile Strength 40.0 MPa

@Strain 1.00 %,
Temperature -20.0 °C
5800 psi

@Strain 1.00 %,
Temperature -4.00 °F
ISO 527
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing