Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 34.0 - 43.0 MPa @Temperature 20.0 °C |
4930 - 6240 psi @Temperature 68.0 °F |
ASTM D882-80, Method A - 100% |
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |