Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.0 - 24.0 MPa @Temperature 75.0 °C |
2900 - 3480 psi @Temperature 167 °F |
|
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |