Polymer Property : Tensile Strength = 24.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 20.0 - 24.0 MPa

@Temperature 75.0 °C
2900 - 3480 psi

@Temperature 167 °F
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..