Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 115 MPa @Diameter 150 - 300 mm |
16700 psi @Diameter 5.91 - 11.8 in |
|
United Cast Bar Unibar 200 Continuously Cast Iron Offers exceptional machinability and excellent surface finishes, but limited strength and wear resistance. Noise and vibration damping are excellent in this grade.Unibar-200 is not suitable for hard.. |
|||
Tensile Strength | 115 MPa @Temperature -40.0 °C |
16700 psi @Temperature -40.0 °F |
ISO 527 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |