Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 75.0 MPa @Strain 2.00 %, Temperature 23.0 °C |
10900 psi @Strain 2.00 %, Temperature 73.4 °F |
50mm/min |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Tensile Strength | 75.0 MPa @Strain 5.00 %, Temperature 60.0 °C |
10900 psi @Strain 5.00 %, Temperature 140 °F |
50mm/min |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Tensile Strength | 75.0 MPa @Strain 6.00 %, Temperature 100 °C |
10900 psi @Strain 6.00 %, Temperature 212 °F |
5mm/min |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength | 75.0 MPa @Temperature 100 °C |
10900 psi @Temperature 212 °F |
ISO 527 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |