Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 236F4Q32 Nylon 6.6, 20% Glass Fiber SAXAMID 236 F4Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers and very good flow properties. It is suitable for applications requiring toughness in co.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide PF006IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF006IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X R2005-30V)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide PF006IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF006IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X R2005-30V)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL RM PA6.6, 30% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |