Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1U |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 0.000 °C |
20.0 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eU |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 120 °C |
20.0 ft-lb/in² @Temperature 248 °F |
ISO 179/1eU |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |