Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 59.0 kJ/m² @Temperature 23.0 °C |
28.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Izod Impact, Unnotched (ISO) | 59.0 kJ/m² @Temperature 0.000 °C |
28.1 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eU |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |