Polymer Property : Izod Impact, Unnotched (ISO) = 15.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 33.0 kJ/m²

@Temperature 23.0 °C
15.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Cycoloy® C4215HF PC+ABS (Europe-Africa-Middle East)
Cycoloy C4215HF is a 15% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic apprearance. It combines good processability with a low s..
Izod Impact, Unnotched (ISO) 33.0 kJ/m²

@Temperature 23.0 °C
15.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Izod Impact, Unnotched (ISO) 33.0 kJ/m²

@Temperature -30.0 °C
15.7 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.