Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00140 GPa | 0.203 ksi | parallel to grain |
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |
|||
Modulus of Rupture | 0.00140 GPa | 0.203 ksi | parallel to thickness |
Zircar Refractory Composites RSBD-LD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-LD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Modulus of Rupture | 0.00140 GPa @Temperature 1260 °C |
0.203 ksi @Temperature 2300 °F |
ASTM C268 |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Modulus of Rupture | 0.00140 GPa @Temperature 540 °C |
0.203 ksi @Temperature 1000 °F |
Fired; ASTM C268 |
BNZ Materials Blazecrete 2800 Dense Castable Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur.. |
|||
Modulus of Rupture | 0.00140 GPa @Temperature 1095 °C |
0.203 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Blazecrete 2800 Dense Castable Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur.. |
|||
Modulus of Rupture | 0.00140 GPa @Temperature 104 °C |
0.203 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Modulus of Rupture | 0.00140 GPa @Temperature 1260 °C |
0.203 ksi @Temperature 2300 °F |
ASTM C268 |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Modulus of Rupture | 0.00140 GPa | 0.203 ksi | ASTM C133 |
BNZ Materials BNZ-26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Modulus of Rupture | 0.00140 GPa | 0.203 ksi | ASTM C133 |
BNZ Materials C-22 Z Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |