Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000800 GPa | 0.116 ksi | EN 993-6: 1995 |
Skamol Group SKAMOLEX V-1100 (475) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Modulus of Rupture | 0.000800 GPa | 0.116 ksi | EN 993-6: 1995 |
Skamol Group V-1100 475 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Modulus of Rupture | 0.000800 GPa | 0.116 ksi | ASTM C133 |
BNZ Materials BNZ-24 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |