Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00117 GPa | 0.170 ksi | Fired (24 hrs at cont. use) |
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |