Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 9.13 MPa @Strain 0.200 %, Temperature 23.0 °C |
1320 psi @Strain 0.200 %, Temperature 73.4 °F |
ASTM D695 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Compressive Strength | 9.13 MPa @Strain 0.200 %, Temperature 23.0 °C |
1320 psi @Strain 0.200 %, Temperature 73.4 °F |
ASTM D695 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |