Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 44.0 MPa @Strain 2 % |
6380 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Compressive Strength | 44.0 MPa @Strain 2 % |
6380 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Compressive Strength | 44.0 MPa @Strain 1 % |
6380 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |
|||
Compressive Strength | 44.0 MPa @Strain 1 % |
6380 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |