Mechanical Properties Metric English Comments
Compressive Strength 379 MPa

@Temperature 138 °C
55000 psi

@Temperature 280 °F
Dry, Autoclave with Post-Cure; ASTM D695
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Compressive Strength 379 MPa

@Temperature 71.1 °C
55000 psi

@Temperature 160 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Strength 379 MPa

@Temperature 288 °C
55000 psi

@Temperature 550 °F
Dry; ASTM D6641
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..