Mechanical Properties Metric English Comments
Compressive Strength 50.0 MPa

@Temperature 250 °C
7250 psi

@Temperature 482 °F
ISO 604
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Compressive Strength 50.0 MPa

@Temperature 250 °C
7250 psi

@Temperature 482 °F
ISO 604
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 170 Dense Refractory Castable
Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 1300 °C
7250 - 8700 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 170 Dense Refractory Castable
Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 170 GM Dense Refractory Castable
Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 1300 °C
7250 - 8700 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 170 GM Dense Refractory Castable
Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 Dense Refractory Castable
Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products...
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 Dense Refractory Castable
Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni..
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 100 C Dense Refractory Castable
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values ..