Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 379 MPa @Temperature 138 °C |
55000 psi @Temperature 280 °F |
Dry, Autoclave with Post-Cure; ASTM D695 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Compressive Strength | 379 MPa @Temperature 71.1 °C |
55000 psi @Temperature 160 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 379 MPa @Temperature 288 °C |
55000 psi @Temperature 550 °F |
Dry; ASTM D6641 |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |