Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 33.0 MPa @Strain 1 % |
4790 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Compressive Strength | 33.0 MPa @Strain 1 % |
4790 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Compressive Strength | 33.0 MPa @Strain 5 % |
4790 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Compressive Strength | 33.0 MPa @Strain 1 % |
4790 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |