Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 114 MPa @Strain 5 % |
16500 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |