Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 105 MPa @Strain 5 % |
15200 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Compressive Strength | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
Compressive Strength | 105 - 115 MPa @Temperature 1300 °C |
15200 - 16700 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |
|||
Compressive Strength | 105 - 115 MPa @Temperature 100 °C |
15200 - 16700 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |