Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.5520 MPa @Strain 25.0 % |
80.06 psi @Strain 25.0 % |
ASTM D3575 |
Sekisui PIOCELAN LSP-15DB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |