Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.115 MPa @Strain 25.0 % |
16.7 psi @Strain 25.0 % |
DIN-EN 826 |
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Compressive Strength | 0.115 MPa @Strain 10.0 % |
16.7 psi @Strain 10.0 % |
DIN-EN 826 |
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |