Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.80 GPa @Temperature 150 °C |
986 ksi @Temperature 302 °F |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 6.80 GPa @Temperature 90.0 °C |
986 ksi @Temperature 194 °F |
|
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa.. |
|||
Tensile Modulus | 6.80 GPa @Temperature 120 °C |
986 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 6.80 GPa @Temperature 60.0 °C |
986 ksi @Temperature 140 °F |
|
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 6.80 GPa @Temperature 90.0 °C |
986 ksi @Temperature 194 °F |
|
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 6.80 GPa @Temperature 60.0 °C |
986 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica.. |
|||
Tensile Modulus | 6.80 GPa @Temperature 23.0 °C |
986 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
(Unverified Data**) Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po.. |
|||
Tensile Modulus | 6.80 GPa @Temperature 23.0 °C |
986 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |