Mechanical Properties Metric English Comments
Tensile Modulus 6.60 GPa

@Temperature 23.0 °C
957 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66  (Unverified Data**)
Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Tensile Modulus 6.60 GPa

@Temperature 90.0 °C
957 ksi

@Temperature 194 °F
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 12 (PA12) based compound. Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 6.60 GPa

@Temperature 90.0 °C
957 ksi

@Temperature 194 °F
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
Tensile Modulus 6.60 GPa

@Temperature 23.0 °C
957 ksi

@Temperature 73.4 °F
LATI Latamid 12 H2 G/30 PA 12, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 12 (PA12) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 6.60 GPa

@Temperature 120 °C
957 ksi

@Temperature 248 °F
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 6.60 GPa

@Temperature 23.0 °C
957 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610  (Unverified Data**)
Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia..
Tensile Modulus 6.60 GPa

@Temperature 23.0 °C
957 ksi

@Temperature 73.4 °F
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..