Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 841 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66  (Unverified Data**)
Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Tensile Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 5.80 GPa

@Temperature 150 °C
841 ksi

@Temperature 302 °F
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Tensile Modulus 5.80 GPa

@Temperature 60.0 °C
841 ksi

@Temperature 140 °F
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 5.80 GPa

@Temperature 90.0 °C
841 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 5.80 GPa

@Temperature 150 °C
841 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 5.80 GPa

@Temperature 120 °C
841 ksi

@Temperature 248 °F
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Modulus 5.80 GPa

@Temperature 90.0 °C
841 ksi

@Temperature 194 °F
LATI Laril 13 G/20 PPOm, 20% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 5.80 GPa

@Temperature 60.0 °C
841 ksi

@Temperature 140 °F
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;..
Tensile Modulus 5.80 GPa

@Temperature 120 °C
841 ksi

@Temperature 248 °F
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Modulus 5.80 GPa

@Temperature 150 °C
841 ksi

@Temperature 302 °F
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 5.80 GPa

@Temperature 120 °C
841 ksi

@Temperature 248 °F
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..