Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.50 GPa @Temperature 23.0 °C |
1230 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 120 °C |
1230 ksi @Temperature 248 °F |
|
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 8.50 GPa @Temperature 60.0 °C |
1230 ksi @Temperature 140 °F |
|
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 60.0 °C |
1230 ksi @Temperature 140 °F |
|
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 60.0 °C |
1230 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 60.0 °C |
1230 ksi @Temperature 140 °F |
|
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 8.50 GPa @Temperature 90.0 °C |
1230 ksi @Temperature 194 °F |
|
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 60.0 °C |
1230 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 23.0 °C |
1230 ksi @Temperature 73.4 °F |
|
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 23.0 °C |
1230 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
(Unverified Data**) Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po.. |