Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.10 GPa @Temperature 23.0 °C |
740 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by .. |
|||
Tensile Modulus | 5.10 GPa @Temperature 23.0 °C |
740 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.10 GPa @Temperature 120 °C |
740 ksi @Temperature 248 °F |
|
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 90.0 °C |
740 ksi @Temperature 194 °F |
|
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Tensile Modulus | 5.10 GPa @Temperature 90.0 °C |
740 ksi @Temperature 194 °F |
|
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 90.0 °C |
740 ksi @Temperature 194 °F |
|
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 150 °C |
740 ksi @Temperature 302 °F |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 90.0 °C |
740 ksi @Temperature 194 °F |
|
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 23.0 °C |
740 ksi @Temperature 73.4 °F |
|
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 23.0 °C |
740 ksi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber Information provided by HexCel |
|||
Tensile Modulus | 5.10 GPa @Temperature 23.0 °C |
740 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |