Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.20 GPa @Temperature 23.0 °C |
1040 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 7.20 GPa @Temperature 150 °C |
1040 ksi @Temperature 302 °F |
|
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 150 °C |
1040 ksi @Temperature 302 °F |
|
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 60.0 °C |
1040 ksi @Temperature 140 °F |
|
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 90.0 °C |
1040 ksi @Temperature 194 °F |
|
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 60.0 °C |
1040 ksi @Temperature 140 °F |
|
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 23.0 °C |
1040 ksi @Temperature 73.4 °F |
|
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 7.20 GPa @Temperature 60.0 °C |
1040 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 60.0 °C |
1040 ksi @Temperature 140 °F |
|
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 23.0 °C |
1040 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |